Another batch is drying.
So easy to make.
Grade 5 titanium and PA6-CF plus some 1.5 mm stainless rods.
What do you make your levers out of?
I’m experimenting with both PLA+ and PA6-CF
I had a PLA+ one last 450 rounds before it got too hot and warped.
Havent gotten enough testing on the CF one yet.
o/ Hi, sorry to bug you: could you reply to this comment? I’m testing a thing and want to make sure I haven’t broken federation.
Ping pong. Not bugging us at all :)
Hell yeah. I got this one promptly and along with your vote activity (comment was at 1 score, not 0) so it absolutely feels like things are working fine right now.
Preciate the ping <3
Nevermind, I can just do this from the other end via my own account lol
Pog
I gotta make sum man they look good
Agreed. Super easy to put together and cheap.
Who are these sailing under?