First time printing PA6-CF
First time printing PA6-CF
I'd like to evolve from PLA+ to PA6-CF. Before I do so, I have some questions I'm hoping some of you that have experience can shed some light on.
My current plan layout is as follows-
- Upgrade 0.4 P1S nozzle and gears to hardened steel
- Change build plate to darkmoon carbon fiber build plate
- Purchase Sovol SH03 to dry filament at 85C for as long as needed
Past this point I begin scratching my head. What exactly should I do next? Not too experienced with dryers, but I imagine I would need some adapter to connect a second PTFE tube from the dryer to the P1S PTFE tube that sticks out of the back, right? Finally, do I run the dryer while printing? Or do I just use desiccant packets in the dryer to maintain low humidity and print with it off?