Hey guys, I’ve just completed my first prints. The top surfaces and sides came out really good, but the undersides came out a little rough. Especially where supports were, what’s the accepted standards for cleaning these areas up? Sandpaper, files, dremel?
What settings should I be looking at to make my next prints even better in these areas?
My setup: Qidi xplus3 Sunlu PLA + 2.0 (using its default filament profile in orca) @ 230/60 300blkfde’s orca/machine settings. 12 walls, 80% infill. Layer height: .2 Support distances: .19
I appreciate the feedback!


The sides nearest the base I’ve seen those artifacts recently. Too harsh of an overhang angle that supports seldom fix unless they are basically fusing with the model and you use a different material as the support. You can also change the print orientation to minimize the overhangs but with PLA+ you don’t wanna deviate too much from the reccomended. With nylon you can do whatever you want because the layer adhesion is great.